Fig. 4From: Linear viscoelasticity of hot-pressed hybrid poplar relates to densification and to the in situ molecular parameters of celluloseTypical DMA temperature scan of hybrid poplar wood at 1 Hz utilizing 2 °C min−1 heating rate for control (top) and hot-pressed (9 % MC, 250 °C) hybrid poplar sample (bottom) tested in 3-point bending mode along the grainBack to article page