Table 1 Hot-pressing conditions and resulting densification including average specific gravity for control and hot-pressed hybrid poplar samples

From: Linear viscoelasticity of hot-pressed hybrid poplar relates to densification and to the in situ molecular parameters of cellulose

 

Wood moisture content (%)

Pressing temperature (°C)

Oven-dry specific gravity (SG0,OD)

% densification = (SGafter − SGbefore) / SGbefore * 100

Control

–

–

0.35 ± 0.03 C

–

9 %, 150 °C

9

150

0.90 ± 0.06 A

154

9 %, 200 °C

9

200

0.90 ± 0.06 A

153

9 %, 250 °C

9

250

0.80 ± 0.10 A,B

132

0 %, 150 °C

0

150

0.64 ± 0.16 B

81

0 %, 200 °C

0

200

0.85 ± 0.12 A

141

0 %, 250 °C

0

250

0.80 ± 0.05 A,B

124

  1. Letters represent Tukey-Kramer grouping